Ecomass® Compound 5100TU96 Tungsten Filled SEBS
Subcategory: Elastomer, TPE; Styrene-Butadiene; Thermoplastic; Styrenic TPE; Polymer
Material Notes: Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applications.- High Specific Gravity
- Tungsten Powder Filled SEBS Base Resin
- Very Flexible
Information provided by Technical Polymers