Ecomass® Compound 705BI79 BaSO4 Filled ABS
Subcategory: ABS Polymer; Thermoplastic; Polymer
Material Notes: Nontoxic alternative to traditional materials, radiation shielding applications.- Moderate Specific Gravity
- BaSO4 Powder Filled ABS
Information provided by Technical Polymers