Ecomass® Compound 705ZC75 Stainless Steel Filled ABS
Subcategory: ABS Polymer; Thermoplastic; Polymer
Material Notes: Nontoxic Alternative to traditional metals, weighting and balancing applications- Moderate Specific Gravity
- Stainless Steel Powder Filled ABS
Information provided by Technical Polymers
| Available Properties |
- Specific Gravity
- Linear Mold Shrinkage
- Tensile Strength at Break
- Elongation at Break
- Flexural Modulus
- Izod Impact, Notched (ISO)
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
|
|
|
|