Ecomass® Compound 1007ZC85 Stainless Steel Filled COPA
Subcategory: Nylon; Thermoplastic; Polymer
Material Notes: Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applications- Stainless Steel Powder Filled Co-Polyamide (COPA)
- Excellent Toughness
Information provided by Technical Polymers
| Available Properties |
- Specific Gravity
- Linear Mold Shrinkage
- Tensile Strength at Break
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Izod Impact, Notched (ISO)
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
|
|
|
|