|   Ecomass® Compound 1080ZB92 Filled Polyamide  Subcategory: Nylon; Thermoplastic; Polymer Material Notes: Nontoxic alternative to Lead (Pb), radiation shielding applications.
 Moderate Specific GravityFilled Polyamide (PA) alloyExcellent Toughness
 Information provided by Technical Polymers 
| | 
    | Available Properties |  
    | Specific GravityLinear Mold ShrinkageTensile Strength, UltimateElongation at BreakTensile ModulusFlexural ModulusFlexural StrengthIzod Impact, NotchedDeflection Temperature at 0.46 MPa (66 psi)Deflection Temperature at 1.8 MPa (264 psi)Melt TemperatureMold TemperatureDrying TemperatureDry Time
 | 
 | 
 |  | | 
    | Property Data |  
    | 