|   Ecomass® Compound 4450CI86 Carbonyl Iron Filled Polypropylene  Subcategory: Polypropylene; Thermoplastic; Polymer Material Notes: Nontoxic alternative to Lead (Pb), for shielding applications
 High Specific GravityCarbonyl Iron Filled Polypropylene Random Co-Polymer
 
| | 
    | Available Properties |  
    | Specific GravityLinear Mold ShrinkageTensile Strength at BreakElongation at BreakFlexural ModulusIzod Impact, Notched (ISO)Deflection Temperature at 0.46 MPa (66 psi)Melt TemperatureMold Temperature
 | 
 | 
 |  | | 