|   Rotuba Ethyl Cellulose 860H2  Subcategory: Cellulosic; Thermoplastic Close Analogs: Eleven grades of Rotuba ethyl cellulose are listed in MatWeb. Data provided by the manufacturer. Key Words: Rotuba Plastics; Cellulosic 
| | 
    | Available Properties |  
    | DensityHardness, Rockwell RTensile Strength, UltimateElongation at BreakIzod Impact, NotchedIzod Impact, Notched, Low TempDielectric ConstantDielectric Constant, Low FrequencyDissipation FactorDissipation Factor, Low FrequencyMelting PointDeflection Temperature at 0.46 MPa (66 psi)
 | 
 | 
 |  | | 
    | Property Data |  
    | 