NOVA Chemicals Novapol® LF-0224-A LDPE
Subcategory: Polyethylene; Thermoplastic; LDPE; Polymer
Close Analogs: This grade no longer in product line
Material Notes: Puncture value is 43.2 J/mm. LDPE. Excellent stiffness, moderate toughness, easy processability. Additive Package: Base Resin. Applications: Industrial packaging, liners, blends with LLDPE, foam articles. Film properties are typical of 38 µm blown film extruded at a blow-up ratio of 2.5:1, but depend on operating conditions. Information supplied by the manufacturer.
| Available Properties |
- Density
- Thickness
- Melt Flow
- Film Tensile Strength at Yield, MD
- Film Tensile Strength at Yield, TD
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Secant Modulus, MD
- Secant Modulus, TD
- Coefficient of Friction
- Elmendorf Tear Strength, MD
- Elmendorf Tear Strength, TD
- Dart Drop
- Haze
- Gloss
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|