NOVA Chemicals Sclair® 12J1 Octene LLDPE Film Resin
Subcategory: Polyethylene; Thermoplastic; LLDPE; Polymer
Key Words: Linear Low Density Polyethylene; Polyoctene; Polyolefin
Material Notes: Film Properties. Features: Low gel, high clarity. Applications: Overwrap, lamination. Data provided by the manufacturer.
| Available Properties |
- Density
- Moisture Vapor Transmission
- Melt Flow
- Hardness, Shore D
- Film Tensile Strength at Yield, MD
- Film Tensile Strength at Yield, TD
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Secant Modulus, MD
- Secant Modulus, TD
- Coefficient of Friction
- Elmendorf Tear Strength, MD
- Elmendorf Tear Strength, TD
- Dart Drop
- Vicat Softening Point
- Brittleness Temperature
- Haze
- Gloss
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|