NOVA Chemicals Sclair® 35BPM MDPE Extrusion Resin, 2.2% Carbon Black Filled
Subcategory: Polyethylene; Thermoplastic; MDPE; Polymer
Key Words: Medium Density Polyethylene
Material Notes: Features: Excellent ESCR, medium molecular weight, good processability, excellent long term thermal stability, good chemical resistance, excellent UV stability. Applications: Extrusion on to metal pipe to produce a corrosion resistant coating for buried pipe systems. Data provided by the manufacturer.
| Available Properties |
- Density
- Water Absorption
- Environmental Stress Crack Resistance
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Melting Point
- Vicat Softening Point
- Brittleness Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|