NOVA Chemicals Sclair® 51-35BP HDPE Extrusion Resin
Subcategory: Polyethylene; Thermoplastic; HDPE
Key Words: High Density Polyethylene
Material Notes: Features: Medium molecular weight, excellent ESCR, excellent toughness, good processability, good chemical resistance. Applications: Extrusion on to metal pipes to produce a corrosion resistant coating for buried pipe systems. Data provided by the manufacturer.
| Available Properties |
- Density
- Environmental Stress Crack Resistance
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Electrical Resistivity
- Dielectric Constant
- Dissipation Factor
- Melting Point
- Vicat Softening Point
- Brittleness Temperature
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|