NOVA Chemicals Sclair® 58G (High Gloss) HDPE Blow Molding Resin
Subcategory: Polyethylene; Thermoplastic; HDPE
Key Words: High Density Polyethylene
Material Notes: Features: Outstanding gloss, pearlescent finish when colored, good processability. Applications: Small part blow molding, injection blow molding, low-moderate ESCR uses. Data provided by the manufacturer.
| Available Properties |
- Density
- Environmental Stress Crack Resistance
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Vicat Softening Point
- Brittleness Temperature
- Processing Temperature
|
|
|
|