NOVA Chemicals Sclair® 61C Octene LLDPE Extrusion Resin
Subcategory: Polyethylene; Thermoplastic; LLDPE
Key Words: Linear Low Density Polyethylene; Polyoctene; Polyolefin
Material Notes: Features: Octene co-polymer, excellent sealability and toughness, high drawdown, high adhesion, good barrier, good abrasion resistance. Applications: Food packaging, milk cartons, paperboard containers. Data provided by the manufacturer.
| Available Properties |
- Density
- Moisture Vapor Transmission
- Melt Flow
- Seal Strength
- Hot Tack Strength
- Processing Temperature
|
|
|
|