NOVA Chemicals Sclair® 97B HDPE Blow Molding Resin
Subcategory: Polyethylene; Thermoplastic; HDPE
Key Words: High Density Polyethylene
Material Notes: Features: Good impact strength, easy processability, high ESCR. Applications: Small part blow molding, high ESCR HIC applications. Data provided by the manufacturer.
| Available Properties |
- Density
- Environmental Stress Crack Resistance
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Vicat Softening Point
- Brittleness Temperature
- Processing Temperature
|
|
|
|