NOVA Chemicals Sclair® 2316 LLDPE Injection Molding Resin
Subcategory: Polyethylene; Thermoplastic; LLDPE
Key Words: Linear Low Density Polyethylene
Material Notes: Features: Low odor, low warpage, fast cycling, high surface gloss, permits light weight lid design.Data provided by the manufacturer.
| Available Properties |
- Density
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Yield
- Flexural Modulus
- Vicat Softening Point
- Brittleness Temperature
- Processing Temperature
|
|
|
|