NOVA Chemicals Sclair® 2714 HDPE Injection Molding Resin
Subcategory: Polyethylene; Thermoplastic; HDPE
Key Words: High Density Polyethylene
Material Notes: Features: Excellent processability for applications requiring good stiffness and toughness, good cold temperature impact properties. Applications: Food containers and lids, frozen food containers. Data provided by the manufacturer.
| Available Properties |
- Density
- Bulk Density
- Melt Flow
- Spiral Flow
- Hardness, Shore D
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Vicat Softening Point
- Brittleness Temperature
- Processing Temperature
|
|
|
|