NOVA Chemicals Sclair® 2717 HDPE Injection Molding Resin
Subcategory: Polyethylene; Thermoplastic; HDPE
Key Words: High Density Polyethylene
Material Notes: Features: Super high flow, good balance of toughness and stiffness, low odor, permits container weight reduction. Applications: Thin walled food containers. Data provided by the manufacturer.
| Available Properties |
- Density
- Apparent Bulk Density
- Melt Flow
- Spiral Flow
- Hardness, Shore D
- Tensile Strength, Yield
- Flexural Modulus
- Vicat Softening Point
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|