NOVA Chemicals Sclair® 2909, 2909-UV8A HDPE Injection Molding Resin
Subcategory: Polyethylene; Thermoplastic; HDPE
Key Words: High Density Polyethylene
Material Notes: Features: High stiffness, maximum impact strength and toughness, good top loading capability, high surface gloss. Applications: Tote boxes, beverage crates. Data provided by the manufacturer.
| Available Properties |
- Density
- Environmental Stress Crack Resistance
- Melt Flow
- Spiral Flow
- Hardness, Shore D
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Vicat Softening Point
- Processing Temperature
|
|
|
|
| Property Data |