NOVA Chemicals Novapol® HB-L455-A HDPE Blow Molding Resin
Subcategory: Polyethylene; Thermoplastic; HDPE
Key Words: High Density Polyethylene
Material Notes: Molded Plaque Properties. Features: excellent processability on high speed, multiple-head blow molding lines, good balance of physical and molding properties. Applications: chemical bottles, toys. Data provided by the manufacturer.
| Available Properties |
- Density
- Environmental Stress Crack Resistance
- Melt Flow
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Izod Impact, Notched
- Processing Temperature
|
|
|
|