NOVA Chemicals Novapol® HE-Y356-A HDPE Extrusion Resin
Subcategory: Polyethylene; Thermoplastic; HDPE
Key Words: High Density Polyethylene
Material Notes: Features: easy processing. Applications: corrugated tubing, profile extrusions, sheet extrusion and thermoforming. Data provided by the manufacturer.
|
|
|