NOVA Chemicals Novapol® LF-0323-B LDPE Film Resin
  Subcategory: Polyethylene; Thermoplastic; LDPE; Polymer; Film 
Key Words: Low Density Polyethylene 
Material Notes:  Film Properties.  Features: General purpose clarity, good heat sealing latitude, easy processability, good drawdown. Applications: Bakery bags, sandwich bags, zipper lock bags, cast film. Data provided by the manufacturer. 
  
  
    | Available Properties | 
   
    
    - Density
 
- Thickness
 
- Melt Flow
 
- Film Tensile Strength at Yield, MD
 
- Film Tensile Strength at Yield, TD
 
- Film Tensile Strength at Break, MD
 
- Film Tensile Strength at Break, TD
 
- Film Elongation at Break, MD
 
- Film Elongation at Break, TD
 
- Secant Modulus, MD
 
- Secant Modulus, TD
 
- Coefficient of Friction
 
- Elmendorf Tear Strength, MD
 
- Elmendorf Tear Strength, TD
 
- Dart Drop
 
- Haze
 
- Gloss
 
- Processing Temperature
 
 
   |   
   |   
 | 
   | 
  
  
    | Property Data | 
   
    
    This page displays only the text 
    of a material data sheet.
  
    To see MatWeb's complete data 
    sheet for this material (including 
    material property data, metal 
    compositions, material suppliers, 
    etc), please click the button below.  | 
   
    | 
    
     | 
    
   |   
 |   
  
   |