Elastomer Engineering Inc E700-70 Polyurethane
Subcategory: Polyester, TP; Polyurethane, TP; Thermoplastic
Material Notes: An extremely tough polyester-based urethane with excellent shock absorbing quality and resistance to abrasion and chemicals. Typical uses: shock deadening pads, abrasion resistant liners and pads, drive rollers, and printing rollers.Information provided by Elastomer Engineering Inc (EEI)
| Available Properties |
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Break
- Tear Strength
|
|
|
|