Elastomer Engineering Inc E850-85A Polyurethane
Subcategory: Polyether; Polyurethane, TP; Thermoplastic
Material Notes: A very tough and cut-resistant polyether-based formulation with good dynamic properties that bonds well to all metals. Information provided by Elastomer Engineering Inc (EEI)
| Available Properties |
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Break
- 100% Modulus
- 300% Modulus
- Rebound
- Tear Strength
- Compression Set
|
|
|
|