Eliokem Sunigum® P95 Acrylate Elastomer
Subcategory: Elastomer, TPE; Thermoplastic
Material Notes: Outstanding heat and UV resistance. Wide range of capabilities. Crosslinked polymer structure. CaCO3 partitioning agent. Can be used in PVC, TPU, TPE/TPO and engineering plastic blends. Used in automotive (interior moldings, decorative profiles/spoilers, interior skins, oil and gas resistant parts), glazing gaskets, roofing membranes, flooring, footwear, cable jacketing, hoses and tubing, overmoldings, appliance gaskets/profiles, and synthetic leather. Information provided by Eliokem.