Emerson & Cuming 2651-1 Stycast® One-Component Epoxy High Service Temp Encapsulant

 

Subcategory: Epoxy; Adhesive; Thermoset

Material Notes:

Features and Typical Applications
Ability to withstand high temperatures, thermal shock, and chemical exposure. These products are designed for heat generating electronic devices which operate in harsh environments. Typical applications include sensors, transformers, power supplies, and rectifiers.

Emerson & Cuming 2651-1 Stycast® One-Component Epoxy High Service Temp Encapsulant

  • Thermally Conductive
  • Good Chemical Resistance
  • Filled
Cure Type: Heat Bonding Type: Epoxy

Available Properties
  • Density
  • Viscosity
  • Hardness, Shore D
  • Dielectric Constant
  • CTE, linear 20°C
  • Thermal Conductivity
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Cure Time
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。