Emerson & Cuming E 1400 Stycast® Two-Component General Purpose Encapsulant
Subcategory: Epoxy; Adhesive; Thermoset
Material Notes:
Features and Typical Applications: Designed as general purpose encapsulants, these products offer a wide range of features including thermal conductivity, mechanical shock and impact resistance, as well as thermal shock protection.
Emerson & Cuming E 1400 Stycast® Two-Component General Purpose Encapsulant
- Good Chemical Resistance
- Filled
- Thermally conductive
- Mix Ratio by Weight = 100:100
Cure Type: Room Temp or Heat Bonding Type: Epoxy
| Available Properties |
- Density
- Viscosity
- Hardness, Shore D
- Dielectric Constant
- Dielectric Strength
- CTE, linear 20°C
- Thermal Conductivity
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Glass Temperature
- Cure Time
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|