Emerson & Cuming 45 Eccobond® Two-Component General Purpose Epoxy Adhesive

 

Subcategory: Epoxy; Adhesive; Thermoset

Material Notes:
Emerson & Cuming 45 Eccobond® Two-Component General Purpose Epoxy Adhesive
Filled, general purpose, room temperature curing, epoxy adhesive and sealant. Flexibility can be adjusted by the amount of Catalyst 15 used. Convenient mix ratio. Good impact resistance. Excellent adhesion to metal, glass and plastic substrates. Mix Ratio of 100:50 to 100:150 (Cat 15 variation). Bonding Type: Epoxy

Available Properties
  • Density
  • Viscosity
  • Adhesive Bond Strength
  • Cure Time
  • Color
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。