Emerson & Cuming 51 Eccobond® Two-Component General Purpose Epoxy Adhesive
Subcategory: Epoxy; Adhesive; Thermoset
Material Notes: Emerson & Cuming 51 Eccobond® Two-Component General Purpose Epoxy Adhesive Filled, general purpose epoxy adhesive. Used with a variety of catalysts. Excellent adhesion to a variety of metal, plastic and ceramic substrates. Mix ratio varies with amount of catalyst used. Bonding Type: Epoxy
| Available Properties |
- Density
- Viscosity
- Adhesive Bond Strength
- Color
|
|
|
|
| Property Data |