Emerson & Cuming 55 Eccobond® Two-Component General Purpose Epoxy Adhesive
Subcategory: Epoxy; Adhesive; Thermoset
Material Notes: Emerson & Cuming 55 Eccobond® Two-Component General Purpose Epoxy Adhesive Unfilled, low viscosity, general purpose, epoxy adhesive. Used with a variety of catalysts. Typical applications include electronic component assembly, staking of adjustment and calibration screws, anchoring of inserts and end filling. Mix ratio varies with amount of catalyst used. Bonding Type: Epoxy