Emerson & Cuming 59C Eccobond® One-Component Silver Filled Electrically Conductive Silicone Adhesive
Subcategory: Silicone; Adhesive; Thermoset
Material Notes: Emerson & Cuming 59C Eccobond® One-Component Silver Filled Electrically Conductive Silicone Adhesive One component, solvent containing, silver filled, electrically conductive, silicone pressure sensitive adhesive. High flexibility. High tack. Bonds formed can be repeatedly opened and sealed. Bonding Type: Silicone
| Available Properties |
- Density
- Adhesive Bond Strength
- Volume Resistivity
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Cure Time
- Color
- Viscosity
|
|
|
|