Emerson & Cuming 83C Eccobond® Two-Component Silver Filled Electrically Conductive Epoxy Adhesive
Subcategory: Epoxy; Adhesive; Thermoset
Material Notes: Emerson & Cuming 83C Eccobond® Two-Component Silver Filled Electrically Conductive Epoxy Adhesive Two component, silver filled, electrically conductive, epoxy adhesive. Smooth, creamy consistency. Good thermal conductivity. Requires heat cure to obtain optimal properties. Easier handling version of Eccobond® 56C with similar properties. Mix ratio of 100:3.5. Cure Type: Heat Bonding Type: Epoxy
| Available Properties |
- Density
- Adhesive Bond Strength
- Volume Resistivity
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Cure Time
- Color
- Viscosity
|
|
|
|
| Property Data |