Emerson & Cuming 64C Eccobond® Two-Component Nickel Filled Electrically Conductive Epoxy Adhesive
Subcategory: Epoxy; Adhesive; Thermoset
Material Notes: Emerson & Cuming 64C Eccobond® Two-Component Nickel Filled Electrically Conductive Epoxy Adhesive Two component, nickel filled, electrically conductive epoxy adhesive. Room temperature cure. Good balance of low cost and high conductivity. Recommended for use where exposure to salt water causes silver based systems to corrode. Cure Type: Room Temperature Bonding Type: Epoxy
| Available Properties |
- Density
- Adhesive Bond Strength
- Volume Resistivity
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Cure Time
- Color
- Viscosity
|
|
|
|