Emerson & Cuming 91 Eccobond® Two-Component High Strength-Peel Epoxy Adhesive
Subcategory: Epoxy; Adhesive; Thermoset
Material Notes: Emerson & Cuming 91 Eccobond® Two-Component High Strength-Peel Epoxy Adhesive Fiberglass filled, medium viscosity, epoxy adhesive with excellent thermal cycling properties. Used with a variety of catalysts. Designed for bonding metals exposed to high stress conditions and for bonding crystals to metals in continuous vibration applications. Mix ratio varies with amount of catalyst used. Bonding Type: Epoxy
| Available Properties |
- Density
- Viscosity
- Adhesive Bond Strength
- Color
|
|
|
|