Emerson & Cuming D 275 Eccobond® One-Component Fast Cure Epoxy Adhesive
Subcategory: Epoxy; Adhesive; Thermoset
Material Notes: Emerson & Cuming D 275 Eccobond® One-Component Fast Cure Epoxy Adhesive Semi-rigid, high strength, fast curing, pourable, epoxy structural adhesive. Good peel strength (12 pli), Recommended for bonding metals, plastics, and ceramics. Cure Type: Heat Bonding Type: Epoxy
| Available Properties |
- Density
- Viscosity
- Adhesive Bond Strength
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Cure Time
- Color
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|