Emerson & Cuming 3193-17 Eccobond® Lighting Epoxy Adhesive
Subcategory: Epoxy; Adhesive; Thermoset
Material Notes: Emerson & Cuming 3193-17 Eccobond® Lighting Epoxy Adhesive One component, heat curing thixotropic epoxy adhesive. 100% solids and elastomer modified. Bonds well to ABS, polycarbonate and other heat sensitive plastics. Recommended for bonding glass headlamps. Cure Type: Heat Bonding Type: Epoxy
| Available Properties |
- Density
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Cure Time
- Color
- Viscosity
|
|
|
|