Emerson & Cuming 23 LV Eccobond® General Purpose Catalyst
Subcategory: Adhesive; Thermoset
Material Notes: Emerson & Cuming 23 LV Eccobond® General Purpose Catalyst Excellent low temperature performance properties, excellent thermal shock/cycle and impact resistance. Best hardener for cryogenic applications. Excellent adhesion to glass. Very low viscosity, low exotherm. Light color good for clear castings. Cure Type: Room Temp or Heat
| Available Properties |
- Density
- Viscosity
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Cure Time
- Pot Life
- Color
|
|
|
|