Emerson & Cuming 24 LV Eccobond® General Purpose Catalyst
Subcategory: Adhesive; Thermoset
Material Notes: Emerson & Cuming 24 LV Eccobond® General Purpose Catalyst Faster curing, shorter working life version of 23 LV. Recommended for small mass castings due to higher exotherm. Cure Type: Room Temp or Heat
| Available Properties |
- Density
- Viscosity
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Cure Time
- Pot Life
- Color
|
|
|
|