Polimeri Europa Extir Leonardo B 3000 AE Expandable Polystyrene

 

Subcategory: Polystyrene; Thermoplastic

Material Notes:
Extir B 3000 AE is a flame retardant expandable polystyrene in the form of spherical beads of medium particle size, containing pentane as blowing agent. Extir does not contain CFC or HCFC. This grade is characterised by fast moulding cycles, good fusion and low energy needs combined with a high mechanical strength and a good surface finishing. Extir B 3000 AE is used for production of shaped mouldings with section greater than 8 mm or medium-high density blocks.

Applications: Extir B 3000 AE is used mainly in building and industrial packaging applications where, for legislative or safety reasons, the use of a flame retardant material is required. Extir B 3000 AE is also suitable for the production of skin moulded items. Typical applications are: • industrial packaging (e.g. cathode ray tube protection) • medium-high density blocks for thermal insulation • moulded panels for underfloor heating • moulded, insulating drainage panels • moulded or block-cut building components

It is recommended to keep the product in a dry well ventilated store between 15-20°C. For product packaged in octabins the guaranteed shelf-life is one month; product in steel drums has a six months guaranteed shelf-life. During the processing of Expandable Polystyrene any sparkle or flame must be avoided and smoking should be forbidden. An adequate electrical grounding of machinery and of pneumatic transport lines is recommended. For further information concerning storage, packaging and processing precautions please refer to "Styrenics - Technical data sheets" and to the "Extir Safety Data Sheet". Regarding "flame retardant" properties, articles made from Extir AE are officially certified “B1 nach DIN 4102”. The action of the flame retardant additive is exerted only after the elimination of blowing agent and, therefore, only after Extir AE has been transformed into foamed articles (suitably aged where necessary).

Processing: Extir B 3000 AE can be easily pre-expanded over a wide density range from 17 to 35 kg/m³. The recommended ageing time before moulding obviously depends on the preexpanded density and ranges from 4 to 48 hours. Extir B 3000 AE can be moulded both on shape or block moulding machines.

Information provided by Polimeri Europa

Available Properties
  • Density
  • Bulk Density
  • Apparent Bulk Density
  • Particle Size
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。