Polimeri Europa Extir EH 3000 Expandable Polystyrene

 

Subcategory: Polystyrene; Thermoplastic

Material Notes:
Extir EH 3000 is an expandable polystyrene in the form of spherical beads of medium particle size, with a low pentane content as blowing agent. Extir does not contain CFC or HCFC. Extir EH 3000 is used for the very fast cycle production of shape mouldings and block moulding with a medium to very high density. It is also characterised by very short maturing time, even at very high density, excellent moulding processability, good fusion, good surface finishing and a very good dimensional stability.

Applications: Extir EH 3000 is a very fast cycling grade used for production of moulded items with wall sections greater than 8 mm and also of skin moulded articles. It can also be used for the production of medium / high density blocks. Finished products exhibit high fusion, high resistance to impact / mechanical stress, and an outstanding dimensional stability. Extir EH 3000 is suitable for the production of food packaging and for food contact applications. Typical applications are: • industrial and protection packaging • internal shells for motorcycle and bicycle crash helmets • containers and loaders for automated manufacturing in the electronics sector • returnable packaging and pallets • medium-high density blocks for thermal insulation

It is recommended to keep the product in a dry well ventilated store between 15-20°C. For product packaged in octabins the guaranteed shelf-life is one month; product in steel drums has a six months guaranteed shelf-life. During the processing of Expandable Polystyrene any sparkle or flame must be avoided and smoking should be forbidden. An adequate electrical grounding of machinery and of pneumatic transport lines is recommended. For further information concerning storage, packaging and processing precautions please refer to "Styrenics - Technical data sheets" and to the "Extir Safety Data Sheet". This grade complies by composition with the requirements set by the main regulations for plastics intended for food contact (including the EEC directive 90/128).

Processing: Extir EH 3000 can be easily pre-expanded on conventional equipment over a wide density range (from 19 to 80 kg/m³), despite its low pentane content. This product needs minimum maturation times (from 1 to 48 hours), even at high density. Moreover the steaming cycle is nearly not influenced by the maturation time. Due to its excellent processability and low pentane content, it is possible to operate with very fast cycle times (mainly by reducing the cooling times) and with low steam pressures. Moulded items and blocks exhibit a very high fusion level, excellent surface aspect, good mechanical properties and an excellent dimensional stability. Extir EH 3000 can be moulded on all types of shape and block moulding machines. Blocks are cut into sheets of the required thickness by means of hot and/or oscillating wires (installation of an exhaust system to remove fumes and dust is recommended).

Information provided by Polimeri Europa

Available Properties
  • Density
  • Bulk Density
  • Apparent Bulk Density
  • Particle Size
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。