Polimeri Europa Edistir N 1782 Polystyrene
Subcategory: Polystyrene; Thermoplastic
Material Notes: General purpose polystyrene with good flow and high heat resistance. Suggested for direct gassing extrusion of heavy gage insulating boards (XPS) and in blend with high concentration of clear SBS for improving clarity and stiffness of the sheets. Designation: Thermoplastics ISO 1622-PS,E,105-06 Applications: Designed for insulation panels (XPS), clear sheets and thermoformed clear packaging. N 1782 is certified UL94 HB "all colors" at 1.5 mm (UL file E83071).This grade in its natural version complies by composition with the requirements set by the main Regulations for plastic materials intended for food contact (including the EEC Directive 90/128 and subsequent amendments). Information provided by Polimeri Europa
| Available Properties |
- Density
- Bulk Density
- Water Absorption
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Rockwell M
- Tensile Strength at Break
- Elongation at Break
- Tensile Modulus
- Flexural Strength
- Izod Impact, Notched (ISO)
- Volume Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- Comparative Tracking Index
- CTE, linear 20°C
- Thermal Conductivity
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
- Glow Wire Test
- Melt Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|