Polimeri Europa Edistir N 2982 Polystyrene
Subcategory: Polystyrene; Thermoplastic
Material Notes: General purpose polystyrene with very high flow and high heat resistance. Special grade for direct gassing extrusion of heavy gage insulating boards (XPS) foamed by blowing agents alternative to CFC and HCFC. Low viscosity process-aid and modifyer for compounding. Designation: Thermoplastics ISO 1622-PS,E,105-20 Applications: XPS insulation panels with improved environmental compatibility. Carrier for masterbatch. Modifyer for thermoplastic elastomers and rubbers (shoe soles, cable extrusion-coating). N 2982 is certified UL94 HB "all colors" at 1.5 mm (UL file E83071). This grade in its natural version complies by composition with the requirements set by the main Regulations for plastic materials intended for food contact (including the EEC Directive 90/128 and subsequent amendments). Information provided by Polimeri Europa
| Available Properties |
- Density
- Bulk Density
- Water Absorption
- Melt Flow
- Tensile Strength at Break
- Elongation at Break
- Tensile Modulus
- Flexural Strength
- CTE, linear 20°C
- Thermal Conductivity
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
- Melt Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|