Polimeri Europa Edistir R 321P Polystyrene
Subcategory: Polystyrene; Thermoplastic
Close Analogs: R321P
Material Notes: Medium impact polystyrene combining easy flow and high stiffness. For injection moulding of parts with low thickness and high rigidity. Designation: Thermoplastics ISO 2897-PS-I,M,083-12-04-30 Applications: Typical uses are toys, stationery, small containers for packaging, refrigerator components, point of sales, household wares, disposable razors, technical items. R 321P is certified UL94 HB "all colors" at 1.5 mm (UL file E83071). This grade in its natural version complies by composition with the requirements set by the main Regulations for plastic materials intended for food contact (including the EEC Directive 90/128 and subsequent amendments). Information provided by Polimeri Europa
| Available Properties |
- Density
- Bulk Density
- Water Absorption
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Rockwell L
- Tensile Strength at Break
- Tensile Strength, Yield
- Elongation at Break
- Tensile Modulus
- Flexural Strength
- Izod Impact, Notched (ISO)
- Izod Impact, Notched
- Volume Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- Comparative Tracking Index
- CTE, linear 20°C
- Thermal Conductivity
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
- Glow Wire Test
- Melt Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|