Polimeri Europa Edistir R 540E Polystyrene
Subcategory: Polystyrene; Thermoplastic
Close Analogs: R540E
Material Notes: HIPS with high stiffness, matt surface finish and good heat resistance. Suitable for general extrusion of thick sheets and profiles. Also used for injection
moldings. Designation: Thermoplastics ISO 2897-PS-I,G,093-03-07-18 Applications: To be used in industrial panels for appliances and buildings. Injection molding of
shoe heels. R 540E satisfies UL94 HB at 1.5 mm (internal test).
This grade in natural version complies by composition with the requirements set
by the main Regulations for plastic materials intended for food contact (included
the EEC Directive 90/128 and following amendments). Information provided by Polimeri Europa
| Available Properties |
- Density
- Bulk Density
- Water Absorption
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Rockwell L
- Tensile Strength at Break
- Tensile Strength, Yield
- Elongation at Break
- Tensile Modulus
- Flexural Strength
- Izod Impact, Notched (ISO)
- Izod Impact, Notched
- Volume Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- Comparative Tracking Index
- CTE, linear 20°C
- Thermal Conductivity
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
- Glow Wire Test
- Melt Temperature
- Mold Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|