Polimeri Europa Edistir R 850E Polystyrene
Subcategory: Polystyrene; Thermoplastic
Close Analogs: R850E
Material Notes: Super high impact polystyrene with good heat resistance. Designed for sheet extrusion and thermoforming of deep drawn containers even
diluted with high percentage of GP. Suitable for general injection molding of tough
medium-walled articles. Designation: Thermoplastics ISO 2897-PS-I,G,093-03-10-18 Applications: Typical uses are thermoformed food packaging as disposable tumblers, flatwares, yoghurt cups, lids. Injection molding of technical items, shoe heels, reels. R 850E is certified UL94 HB "all colors" at 1.5 mm (UL file E83071).
This grade in natural version complies by composition with the requirements set
by the main Regulations for plastic materials intended for food contact (included
the EEC Directive 90/128 and following amendments). Information provided by Polimeri Europa
| Available Properties |
- Density
- Bulk Density
- Water Absorption
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Rockwell L
- Tensile Strength at Break
- Tensile Strength, Yield
- Elongation at Break
- Tensile Modulus
- Flexural Strength
- Izod Impact, Notched (ISO)
- Izod Impact, Notched
- Volume Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- Comparative Tracking Index
- CTE, linear 20°C
- Thermal Conductivity
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
- Glow Wire Test
- Melt Temperature
- Mold Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|