Polimeri Europa Edistir RK 5512G Polystyrene
Subcategory: Polystyrene; Thermoplastic
Close Analogs: RK5512G
Material Notes: UL94 V-2, polybromobiphenylether (PBBE) free, high impact polystyrene with good mechanical and thermal properties. It exhibits a good stability to the processing conditions and to the light
exposure. This grade is recommended for injection moulding in the electronic industry. Designation: Thermoplastics ISO 2897-PS-I,M,088-06-07-23 Applications: TV back covers, computer housings, printers and copiers. This grade is certified UL94 V-2 at 1.5mm "all colors" (UL file E83071). RK 5512G may be supplied in natural or colored version upon request. Information provided by Polimeri Europa
| Available Properties |
- Density
- Bulk Density
- Water Absorption
- Linear Mold Shrinkage
- Melt Flow
- Tensile Strength at Break
- Tensile Strength, Yield
- Elongation at Break
- Tensile Modulus
- Flexural Strength
- Izod Impact, Notched (ISO)
- Izod Impact, Notched
- Volume Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- Comparative Tracking Index
- CTE, linear 20°C
- Thermal Conductivity
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
- Glow Wire Test
- Melt Temperature
- Drying Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|