Polimeri Europa Edistir ICE S 800/N Polystyrene

 

Subcategory: Polystyrene; Thermoplastic

Close Analogs: S800/N

Material Notes:
Very high environmental stress cracking resistant (VH ESCR) modified HIPS. ICE S 800/N exhibits high toughness and excellent chemical resistance to oils, fats and chemical agents and in particular to cyclopentane.

Designation: Thermoplastics ISO 2897-PS-I,G,093-06-07-12

Applications: Designed for inner liners and frames for refrigerators where cyclopentane is used as blowing agent for insulating polyurethane foams. ICE S 800/N significantly improves the wall thickness distribution in thermoforming and allows to optimize the thickness of the original extruded sheet.

ICE S 800/N satisfies the norm UL94 HB at 1.5 mm (internal test). This grade in its natural version complies by composition with the requirements set by the main Regulations for plastic materials intended for food contact (including the EEC Directive 90/128 and subsequent amendments). ICE S 800/N is supplied in round pellets

Information provided by Polimeri Europa

Available Properties
  • Density
  • Bulk Density
  • Water Absorption
  • Linear Mold Shrinkage
  • Melt Flow
  • Hardness, Rockwell L
  • Tensile Strength at Break
  • Tensile Strength, Yield
  • Elongation at Break
  • Tensile Modulus
  • Flexural Strength
  • Izod Impact, Notched (ISO)
  • Izod Impact, Notched
  • Volume Resistivity
  • Surface Resistance
  • Dielectric Constant
  • Dielectric Strength
  • Dissipation Factor
  • Comparative Tracking Index
  • CTE, linear 20°C
  • Thermal Conductivity
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Vicat Softening Point
  • Flammability, UL94
  • Glow Wire Test
  • Melt Temperature
  • Mold Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。