Polimeri Europa EDISTIR PD RK4514H High Impact Polystyrene (HIPS)
Subcategory: Polystyrene; Thermoplastic
Close Analogs: Polimeri Europa now has Enichem's plastics businesses. This grade is no longer in the product line.
Material Notes: Symbol according to ISO 1043-1: S/B Designation: Thermoplastic ISO 2897-SB,M,093-06-07-23 UL94 V-2, polybromodiphenylether (PBBE) free, antimony free, HIPS satisfying at 960°C the glow wire test (GWT) acc. DIN/IEC 695-2-1. This product is suggested for injection molding where exhibits good flow, good mechanical and thermal properties and enhanced UV stability. Applications: Developed for fuse and circuit breaker boxes, cable junction boxes and other electrical appliances. Unfilled. Suitable for Injection Molding. Supplied as pellets. Contains release agent. ISO data. Information provided by Enichem
| Available Properties |
- Density
- Melt Flow
- Tensile Strength, Yield
- Elongation at Break
- Tensile Modulus
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- Electrical Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Constant, Low Frequency
- Dielectric Strength
- Dissipation Factor
- Dissipation Factor, Low Frequency
- Comparative Tracking Index
- Vicat Softening Point
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|