Polimeri Europa KOBLEND PCA PD 935 G4 PC+ABS, 20% Glass Fiber
Subcategory: Polycarbonate; ABS Polymer; Thermoplastic; Polymer
Close Analogs: Polimeri Europa now has Enichem's plastics businesses. This grade is no longer in the product line.
Key Words: Poly(Acrylonitrile Butadiene Styrene) + Polycarbonate
Material Notes: Symbol according to ISO 1043/1/2: PC+ABS (GF) Injection moulding grade, reinforced with 20% glass fibres, high stiffness, very good dimensional stability. Main application fields: structural non aesthetic parts in the automotive industry, electro-mechanical components Filled. Suitable for Injection Molding. Supplied as pellets. ISO data. Information provided by Enichem
| Available Properties |
- Density
- Water Absorption
- Melt Flow
- Tensile Strength, Ultimate
- Elongation at Break
- Tensile Modulus
- Electrical Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Constant, Low Frequency
- Dielectric Strength
- Dissipation Factor
- Dissipation Factor, Low Frequency
- Comparative Tracking Index
- CTE, linear 20°C
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|