Polimeri Europa Sinkral C 442 ABS Resin
Subcategory: ABS Polymer; Thermoplastic
Close Analogs: ISO 2580-ABS 1, MGN, 105-08-16-20
Material Notes: Sinkral C 442 is a heat resistant injection molding grade offering good flow and impact resistance together with excellent thermal stability during processing. Designation: Thermoplastic ISO 2580-ABS 1,MGN,105-08-16-20Applications: Thanks to a low Yellow Index and color constancy, it is suitable for self-coloring, mainly in the automotive industry for interior (extruded profiles, interior trim,..) and with proper masterbatches, for exterior parts such as grilles and rear view mirrors. Grade available either in natural or colored versions. Suitable masterbatches could be recommended for self-coloring. Information provided by Polimeri Europa
| Available Properties |
- Density
- Water Absorption
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched (ISO)
- Charpy Impact Unnotched
- Charpy Impact, Notched
- Izod Impact, Notched
- Volume Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- CTE, linear 20°C
- Thermal Conductivity
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
- Glow Wire Test
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|