Polimeri Europa Sinkral D 232/M3 ABS Resin
Subcategory: ABS Polymer; Thermoplastic
Close Analogs: ISO 2580-ABS 1, EGN, 105-08-09-15
Material Notes: Special low gloss extrusion/ co-extrusion grade, with good flow. Designation: Thermoplastic ISO 2580-ABS 1, EGN, 105-08-09-15Applications: Sinkral D 232-M3 is widely used in the extrusion / co-extrusion of foils, when a very high matt appearance is required, as well as in the extrusion of profiles. This grade is supplied in natural only for self-coloring. Sinkral D 232/M3 meets European Standards for plastics in contact with foods. Information provided by Polimeri Europa
| Available Properties |
- Density
- Water Absorption
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched (ISO)
- Charpy Impact Unnotched
- Charpy Impact, Notched
- Izod Impact, Notched
- Volume Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- CTE, linear 20°C
- Thermal Conductivity
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
- Glow Wire Test
- Melt Temperature
- Drying Temperature
- Dry Time
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|